| Copper ETP (C101) | C11000 · CW004A · Cu-ETP · IS 191 Cu-ETP | Cu ≥ 99.90, O ~0.04 | ≥ 100% IACS conductivity, excellent thermal conductivity, soft & ductile | Busbars, earthing strips, electrical sheets, roofing, heat-transfer components |
| Copper DHP (C106) | C12200 · CW024A · Cu-DHP | Cu ≥ 99.90, P 0.015 – 0.040 | Weldable & brazeable without embrittlement, ~85% IACS | Plumbing & refrigeration tube, heat exchangers, pressure vessels, PVC-coated copper tube |
| Free-Cutting Brass (CZ121) | C36000 · CW614N · CuZn39Pb3 · IS 319 Gr.1 | Cu 58, Pb 3, Zn bal. | 100% machinability rating, good strength | Turned parts, valve bodies, fittings, fasteners, inserts |
| Brass 63/37 & 70/30 | C27200 / C26000 · CW508L / CW505L · CZ108 / CZ106 | Cu 63 or 70, Zn bal. | Deep-drawing (cartridge) quality, bright finish | Sheets, strips, tubes, radiator cores, decorative & architectural work |
| Naval Brass (CZ112) | C46400 · CW712R · CuZn38Sn1 | Cu 60, Sn 1, Zn bal. | Tin addition resists dezincification in seawater | Marine hardware, tube sheets, condenser plates, propeller shafts |
| Aluminium 1100 / 1050 | IS 19000 · EN AW-1100 · A91100 | Al ≥ 99.0 | Highest formability & conductivity among Al grades, excellent corrosion resistance | Chemical equipment, heat-exchanger fins, cladding, reflectors |
| Aluminium 5052-H32 | IS 52000 · EN AW-5052 · A95052 | Mg 2.5, Cr 0.25 | Best weldable marine-grade sheet, good fatigue strength | Boat hulls, tanks, pressure vessels, panels, truck bodies |
| Aluminium 6061-T6 | IS 65032 · EN AW-6061 · A96061 | Mg 1.0, Si 0.6, Cu 0.28, Cr 0.2 | UTS ≈ 310 MPa, heat-treatable, weldable, anodises well | Structural sections, machined parts, jigs & fixtures, automotive |
| Aluminium 6082-T6 (HE30) | IS 64430 · EN AW-6082 · BS HE30 / H30 | Mg 0.9, Si 1.0, Mn 0.7 | Highest strength of the 6000 series (UTS ≈ 340 MPa), good machinability | Bridges, cranes, transport, high-stress structural plate & bar |
| Aluminium 7075-T6 | IS 74530 · EN AW-7075 · A97075 | Zn 5.6, Mg 2.5, Cu 1.6, Cr 0.23 | UTS ≈ 570 MPa – one of the strongest Al alloys | Aerospace, moulds, tooling plates, high-performance components |
| Aluminium 2024-T351 | IS 24345 · EN AW-2024 · A92024 | Cu 4.4, Mg 1.5, Mn 0.6 | High strength & fatigue resistance; limited corrosion resistance (often clad) | Aircraft structures, rivets, precision machined parts |
| Nickel 200 / 201 | N02200 / N02201 · 2.4066 / 2.4068 · LC-Ni 99 | Ni ≥ 99.0 (201: C ≤ 0.02) | Resists caustic alkalis, ferromagnetic; 201 for service above 315 °C | Caustic evaporators, food processing, electronic & electroplating equipment |
| Monel 400 | N04400 · 2.4360 · NiCu30Fe · BS 3072 NA13 | Ni 63, Cu 31, Fe 2.5, Mn 2 | Outstanding in seawater, HF & de-aerated acids; UTS ≈ 550 MPa | Seawater valves & pumps, HF alkylation, heat exchangers, marine fasteners |
| Monel K-500 | N05500 · 2.4375 · NiCu30Al3Ti | Ni 63, Cu 30, Al 2.7, Ti 0.6 | Age-hardenable to UTS ≈ 1100 MPa, non-magnetic, Monel 400 corrosion resistance | Pump & propeller shafts, oil-well tools, springs, fasteners |
| Inconel 600 | N06600 · 2.4816 · NiCr15Fe · BS 3072 NA14 | Ni 72, Cr 15.5, Fe 8 | Oxidation & chloride-SCC resistance to 1100 °C; resists caustic | Furnace muffles, heat-treatment fixtures, nuclear steam generators, chemical plant |
| Inconel 601 | N06601 · 2.4851 · NiCr23Fe | Ni 61, Cr 23, Fe 14, Al 1.4 | Superior oxidation & spalling resistance to 1200 °C | Radiant tubes, furnace baskets, burner components, thermal reactors |
| Inconel 625 | N06625 · 2.4856 · NiCr22Mo9Nb · Gr.1 & Gr.2 | Ni 61, Cr 21.5, Mo 9, Nb 3.6 | Very high strength & fatigue resistance, immune to chloride pitting; cryogenic to 980 °C | Offshore risers, flue-gas scrubbers, aerospace ducting, overlay cladding, bellows |
| Inconel 718 | N07718 · 2.4668 · NiCr19Fe19Nb5Mo3 | Ni 52.5, Cr 19, Fe 18, Nb 5, Mo 3, Ti 0.9 | Precipitation-hardened, UTS ≈ 1240 MPa, usable −250 °C to 700 °C | Gas-turbine discs, downhole tools, high-strength fasteners, cryogenic tanks |
| Incoloy 800 / 800H / 800HT | N08800 / N08810 / N08811 · 1.4876 / 1.4958 / 1.4959 · X10NiCrAlTi32-21 | Ni 32, Cr 21, Fe bal., Al+Ti | Creep-rupture strength & carburisation resistance at 600 – 1000 °C | Reformer & pyrolysis tubes, superheaters, heat-treatment furnaces |
| Incoloy 825 | N08825 · 2.4858 · NiCr21Mo | Ni 42, Cr 21.5, Fe 30, Mo 3, Cu 2.2, Ti 0.9 | Resists sulphuric & phosphoric acids, chloride SCC and pitting | Acid pickling, pollution-control, oil & gas sour-service piping, nuclear fuel reprocessing |
| Hastelloy C-276 | N10276 · 2.4819 · NiMo16Cr15W | Ni 57, Mo 16, Cr 16, W 4, Fe 5 | Broadest resistance to oxidising & reducing media, wet chlorine, hypochlorite | FGD scrubbers, chemical reactors, pulp & paper bleach plants, waste treatment |
| Hastelloy C-22 | N06022 · 2.4602 · NiCr21Mo14W | Ni 56, Cr 22, Mo 13, W 3, Fe 3 | Better than C-276 in oxidising media & crevice conditions; weld-friendly | Pharmaceutical reactors, acid handling, incinerator scrubbers, cellulose acetate plant |
| Hastelloy B-2 / B-3 | N10665 / N10675 · 2.4617 / 2.4600 · NiMo28 | Ni 69, Mo 28, Fe ≤ 2 | Exceptional in hydrochloric acid at all concentrations & temperatures (reducing only) | HCl handling, acetic acid, sulphuric acid at moderate concentration |
| Titanium Gr.1 / Gr.2 | R50250 / R50400 · 3.7025 / 3.7035 · CP Ti | Ti ≥ 99.2 (Gr.2: O ≤ 0.25, Fe ≤ 0.30) | Gr.2: UTS ≥ 345 MPa, density 4.51 g/cm³, immune to seawater & wet chlorine | Condenser tubes, heat exchangers, chlor-alkali cells, desalination, anodes |
| Titanium Gr.5 (Ti-6Al-4V) | R56400 · 3.7165 · TiAl6V4 | Al 6, V 4, Ti bal. | UTS ≥ 895 MPa, heat-treatable, best strength-to-weight ratio | Aerospace & defence, pressure vessels, medical implants, high-performance fasteners |
| Cupro-Nickel 90/10 | C70600 · CW352H · CuNi10Fe1Mn · BS CN102 | Cu 88.6, Ni 10, Fe 1.4, Mn 1 | Seawater corrosion & biofouling resistance, good weldability | Seawater piping, condenser & cooler tubes, desalination, offshore firewater |
| Cupro-Nickel 70/30 | C71500 · CW354H · CuNi30Mn1Fe · BS CN107 | Cu 68, Ni 30, Fe 0.7, Mn 1 | Higher strength & velocity tolerance than 90/10 | High-velocity seawater systems, naval piping, heat-exchanger tubes |
| Aluminium Bronze AB2 | C95800 / C63000 · CC333G / CW307G · CuAl10Ni5Fe4 · IS 305 AB2 | Al 9 – 10, Ni 4.5 – 5, Fe 4, Mn 1 | UTS ≈ 600 – 700 MPa, excellent wear, cavitation & seawater resistance | Pump & valve components, propellers, gears, bushes, wear plates, non-sparking tools |
| Gunmetal LG2 | C83600 · CC491K · CuSn5Zn5Pb5 · IS 318 LTB2 | Cu 85, Sn 5, Zn 5, Pb 5 | Pressure-tight castings, good machinability & bearing properties | Valve bodies, pump casings, bushes, steam fittings, bearings |
| Phosphor Bronze PB1 / PB102 | C51000 / C52100 · CW451K / CW453K · CuSn5 / CuSn8 | Sn 5 – 8, P 0.1 – 0.35 | High fatigue strength, spring quality, low friction | Springs, bearings, bushes, gears, electrical contacts, wear strips |
| Lead & Zinc | Pb 99.97 IS 27 · Zn 99.95 IS 209 | Commercially pure | Lead: radiation shielding & acid resistance; zinc: sacrificial protection | Lead sheets, pipes & linings; zinc anodes, sheets & galvanising |