Seawater & Chlorides
316L · Duplex 2205 · Super Duplex 2507 · Cu-Ni 90/10 · Monel 400 · Titanium Gr 2
Compositions are nominal values (weight %) and properties are typical, for guidance only. Exact limits depend on the product standard, form and condition – always refer to the applicable specification and the mill test certificate supplied with the material.
Iron-chromium alloys with at least 10.5% chromium, which forms a self-healing passive oxide film. Austenitic 200 and 300 series grades offer excellent formability and weldability; martensitic grades (410, 420, 431) can be hardened; ferritic 430 is magnetic and economical; duplex grades combine austenite and ferrite for roughly twice the yield strength of 316 and superior chloride stress-corrosion resistance. Our largest stock family – including PVC-coated 304 and 316 sheet. See the Stainless Steel page for forms and sizes.
| Grade | Equivalents | Nominal Composition | Key Properties | Typical Applications |
|---|---|---|---|---|
| SS 202 Austenitic · Cr-Mn-Ni | UNS S20200 · W.Nr. 1.4373 · SUS 202 | Cr 18 · Mn 8.5 · Ni 5 · N ≤0.25 · C ≤0.15 | Low-nickel austenitic grade with manganese and nitrogen replacing part of the nickel; good strength and formability at lower cost than 304; moderate corrosion resistance. | Utensils, railings and architectural work, automotive trim, storage tanks, indoor applications |
| SS 304 / 304L Austenitic | UNS S30400 / S30403 · W.Nr. 1.4301 / 1.4307 · SUS 304 · IS X04Cr19Ni9 | Cr 18 · Ni 8 · C ≤0.07 (304L ≤0.03) | General-purpose "18/8" stainless; excellent formability and weldability; non-magnetic when annealed. 304L avoids sensitisation after welding. Available PVC-coated for scratch-free fabrication. | Food & dairy equipment, kitchenware, chemical tanks, architectural work, heat exchangers |
| SS 316 / 316L Austenitic | UNS S31600 / S31603 · W.Nr. 1.4401 / 1.4404 · SUS 316 · IS X04Cr17Ni12Mo2 | Cr 17 · Ni 12 · Mo 2.5 · C ≤0.08 (316L ≤0.03) | Molybdenum improves pitting and crevice resistance in chlorides (PREN ≈ 24); good creep strength. Our PVC-coated 316 sheet speciality grade. | Marine fittings, pharmaceutical & chemical plants, pulp & paper, coastal structures |
| SS 316Ti Austenitic · Ti-stabilised | UNS S31635 · W.Nr. 1.4571 · SUS 316Ti | Cr 17 · Ni 12 · Mo 2.2 · Ti ≥5×C | Titanium-stabilised 316 that resists intergranular corrosion after welding or service at 425–815 °C; widely specified on European drawings. | Chemical and process equipment, exhaust systems, welded pressure vessels, heat exchangers |
| SS 321 Austenitic · Ti-stabilised | UNS S32100 · W.Nr. 1.4541 · SUS 321 | Cr 18 · Ni 10 · Ti ≥5×C | Titanium-stabilised 304 for service in the 425–815 °C sensitisation range; good oxidation resistance and creep strength. | Aircraft exhaust manifolds, expansion joints, boiler casings, high-temperature chemical equipment |
| SS 347 Austenitic · Nb-stabilised | UNS S34700 · W.Nr. 1.4550 · SUS 347 | Cr 18 · Ni 11 · Nb ≥10×C | Niobium-stabilised alternative to 321 with slightly better high-temperature strength and weld properties. | Refinery heaters, high-temperature piping, welded chemical plant, aerospace components |
| SS 309 / 309S Austenitic · Heat-resisting | UNS S30900 / S30908 · W.Nr. 1.4828 / 1.4833 | Cr 23 · Ni 13 · C ≤0.20 (309S ≤0.08) | Good oxidation resistance up to about 1000 °C; high-alloy filler for dissimilar welds. | Furnace and boiler components, heat exchangers, dissimilar-metal welding |
| SS 310 / 310S Austenitic · Heat-resisting | UNS S31000 / S31008 · W.Nr. 1.4845 · SUS 310S | Cr 25 · Ni 20 · C ≤0.25 (310S ≤0.08) | Heat-resisting grade with excellent oxidation resistance up to about 1100 °C. | Furnace parts, heat-treatment fixtures, radiant tubes, kiln and burner components |
| SS 410 Martensitic | UNS S41000 · W.Nr. 1.4006 · SUS 410 | Cr 12.5 · C ≤0.15 | Hardenable by heat treatment; magnetic; good strength with moderate corrosion resistance. | Valve trim, pump shafts, turbine parts, fasteners, cutlery |
| SS 420 Martensitic | UNS S42000 · W.Nr. 1.4021 / 1.4028 · SUS 420J1/J2 | Cr 13 · C ≥0.15 | Higher carbon for greater hardness (around 50 HRC when hardened); good wear resistance. | Surgical and dental instruments, cutlery, moulds, pump shafts |
| SS 430 Ferritic | UNS S43000 · W.Nr. 1.4016 · SUS 430 | Cr 17 · C ≤0.12 | Magnetic, non-hardenable; good formability and resistance to mild corrosion; economical. | Appliance panels, automotive trim, sinks, decorative applications |
| SS 431 Martensitic · Ni-bearing | UNS S43100 · W.Nr. 1.4057 · SUS 431 | Cr 16 · Ni 2 · C 0.20 | Highest corrosion resistance of the martensitic grades and high tensile strength after hardening and tempering (about 850–1000 MPa). | Pump and propeller shafts, marine fasteners, valve parts, aircraft fittings |
| SS 904L Super austenitic | UNS N08904 · W.Nr. 1.4539 | Cr 20 · Ni 25 · Mo 4.5 · Cu 1.5 · C ≤0.02 | High-alloy austenitic grade with excellent resistance to sulphuric and phosphoric acids and to chloride pitting (PREN ≈ 35); non-magnetic. | Sulphuric-acid plants, fertiliser and phosphoric-acid equipment, seawater systems, pharmaceutical reactors |
| Duplex 2205 Duplex | UNS S31803 / S32205 · W.Nr. 1.4462 | Cr 22 · Ni 5 · Mo 3 · N 0.17 | About twice the yield strength of 316; excellent chloride stress-corrosion cracking resistance (PREN ≈ 35). | Oil & gas, chemical tankers, desalination, pulp & paper, heat exchangers |
| Super Duplex 2507 Super Duplex | UNS S32750 · W.Nr. 1.4410 | Cr 25 · Ni 7 · Mo 4 · N 0.27 | Very high strength; outstanding pitting and crevice resistance in seawater (PREN ≥ 40). | Offshore platforms, subsea systems, seawater cooling, firewater lines |
Also stocked on request: SS 303 (free-machining), SS 317L, SS 409, SS 416 and SS 440C. PVC / plastic-coated sheets in 304 and 316 are a Honesty Impex speciality.
Plain carbon steels for pressure piping, boilers, vessels and forged piping components – specified by ASTM / ASME for guaranteed chemistry, strength and (where required) impact toughness. Also medium-carbon engineering grades for shafts and machined parts. See the Carbon Steel page.
| Grade | Equivalents | Nominal Composition | Key Properties | Typical Applications |
|---|---|---|---|---|
| A106 Gr. B Seamless pipe · High temp. | ASTM A106 / ASME SA106 Gr. B · UNS K03006 · P265GH (similar) | C ≤0.30 · Mn 0.29–1.06 · Si ≥0.10 | The standard seamless carbon steel pipe for high-temperature service; tensile ≥415 MPa, yield ≥240 MPa; weldable and bendable. | Refinery and power-plant piping, steam lines, boilers, process piping, hydraulic lines |
| A53 Gr. B ERW / seamless pipe | ASTM A53 Gr. B · UNS K03005 · IS 1239 (similar) | C ≤0.30 · Mn ≤1.20 | General-purpose black or hot-dip galvanised pipe; tensile ≥415 MPa, yield ≥240 MPa; threaded, grooved or plain ends. | Water, air and gas lines, fire-fighting systems, structural and mechanical use, low-pressure steam |
| A333 Gr. 6 Low-temperature pipe | ASTM A333 / ASME SA333 Gr. 6 · UNS K03006 | C ≤0.30 · Mn 0.29–1.06 · Si ≥0.10 | Normalised seamless pipe impact tested at −46 °C; tensile ≥415 MPa, yield ≥240 MPa. | LPG and cryogenic piping, cold-climate pipelines, refrigeration plants |
| A105 / A105N Forging | ASTM A105 / ASME SA105 · UNS K03504 · C22.8 (1.0460, similar) | C ≤0.35 · Mn 0.60–1.05 · Si 0.10–0.35 | The standard carbon steel for forged flanges and socket-weld / threaded fittings; tensile ≥485 MPa, yield ≥250 MPa; A105N normalised for improved toughness. | Flanges, forged fittings, olets, valve bodies, piping components |
| A234 WPB Butt-weld fitting | ASTM A234 / ASME SA234 WPB · UNS K03006 | C ≤0.30 · Mn 0.29–1.06 · Si ≥0.10 | Wrought carbon steel fittings matching A106 Gr. B / A53 Gr. B pipe; tensile 415–585 MPa, yield ≥240 MPa. | Elbows, tees, reducers, caps and stub ends for moderate and high-temperature piping |
| A350 LF2 Low-temperature forging | ASTM A350 / ASME SA350 LF2 Cl. 1 · UNS K03011 | C ≤0.30 · Mn 0.60–1.35 · Si 0.15–0.30 | Carbon steel forgings impact-tested at −46 °C; tensile 485–655 MPa, yield ≥250 MPa; often dual-certified with A105. | Low-temperature flanges, fittings and valves for LPG, petrochemical and cold climates |
| A420 WPL6 Low-temperature fitting | ASTM A420 / ASME SA420 WPL6 · UNS K03006 | C ≤0.30 · Mn 0.50–1.35 · Si 0.15–0.40 | Butt-weld fittings impact tested at −46 °C, matching A333 Gr. 6 pipe and A350 LF2 flanges. | Low-temperature process and refrigeration piping, LPG terminals |
| SA 516 Gr. 60 / 70 Boiler quality (BQ) plate | ASTM A516 / ASME SA516 · UNS K02100 / K02700 · IS 2002 Gr. 2 (similar) | C ≤0.27–0.31 (by thickness) · Mn 0.85–1.20 · Si 0.15–0.40 | Carbon steel plate for moderate and lower-temperature pressure service; Gr. 70 tensile 485–620 MPa, yield ≥260 MPa; HIC / normalised options. | Boilers, pressure vessels, storage tanks, heat exchangers, columns |
| SA 210 Gr. A1 / C Boiler tube | ASTM A210 / ASME SA210 · UNS K02707 / K03501 · BS 3059 360/440 | C ≤0.27 (A1) / ≤0.35 (C) · Mn ≤0.93 / 0.29–1.06 | Seamless medium-carbon boiler and superheater tubes; tensile ≥415 MPa (A1), ≥485 MPa (C). | Water-wall, economiser and boiler tubes, heat exchangers |
| A36 Structural | ASTM A36 · UNS K02600 · S275JR / IS 2062 E250 (similar) | C ≤0.26 · Mn 0.80–1.20 · Si ≤0.40 | Carbon structural steel with yield ≥250 MPa and tensile 400–550 MPa; readily welded, bolted and riveted. | Structural plates and sections, base plates, brackets, general fabrication |
| AISI 1018 / 1020 Low carbon bar | SAE 1018 / 1020 · C15 / C22 (1.0401 / 1.0402) · EN 3B (similar) | C 0.18–0.20 · Mn 0.60–0.90 | Low-carbon steel with good weldability and machinability; can be carburised for a hard case. | Shafts, pins, spacers, brackets, machined and fabricated parts |
| C45 / AISI 1045 Medium carbon bar | W.Nr. 1.0503 · SAE 1045 · EN 8 / 080M46 · IS 45C8 · S45C | C 0.45 · Mn 0.65 · Si 0.25 | Medium-carbon steel with tensile about 600–750 MPa normalised; induction or flame hardenable to 55 HRC at the surface. | Shafts, gears, bolts, crankshafts, hydraulic rods, machine parts |
Cr-Mo pressure grades (A335 P11 / P22 / P91, A182 F11 / F22, A387 plates) are listed under Alloy Steel. Structural mild steel grades to IS 2062 are under Mild Steel.
Low-carbon structural and general-engineering steels – the most widely used and economical steels for fabrication, construction and machining. Supplied to Indian (IS), European (EN / DIN) and British (BS 970 "EN" series) standards. See the Mild Steel page.
| Grade | Equivalents | Nominal Composition | Key Properties | Typical Applications |
|---|---|---|---|---|
| IS 2062 E250 Structural · Gr. A / B / BR / B0 | IS 2062:2011 E250 (formerly Fe 410) · S235JR / S275JR (similar) · ASTM A36 (similar) | C ≤0.22 · Mn ≤1.50 · Si ≤0.40 · S, P ≤0.045 | Standard Indian structural steel; yield ≥250 MPa, tensile ≥410 MPa, elongation ≥23%; excellent weldability. Quality B / BR / B0 add impact requirements. | Building and bridge structures, plates, angles, channels, beams, general fabrication |
| IS 2062 E350 High-tensile structural | IS 2062 E350 (formerly Fe 490) · S355JR / S355J0 (similar) | C ≤0.20 · Mn ≤1.55 · Si ≤0.45 · micro-alloyed | Higher strength for lighter sections; yield ≥350 MPa, tensile ≥490 MPa; good weldability with micro-alloy chemistry. | Cranes, heavy structures, earth-moving equipment, transmission towers, wagons |
| IS 1239 (Part 1) MS tubes · Light / Medium / Heavy | IS 1239 Pt 1 · YSt 210 / 240 / 310 · BS 1387 (similar) | C ≤0.20 · Mn ≤1.30 (ERW) | Electric-resistance-welded black or galvanised tubes, ½" to 6" NB, in light (A), medium (B) and heavy (C) classes; threaded or plain ends. | Water and gas lines, fire-fighting, scaffolding, fencing, structural and general-purpose piping |
| IS 1161 Structural tubes | IS 1161 YSt 210 / 240 / 310 · EN 10219 S235 / S275 / S355 (similar) | C ≤0.20–0.25 · Mn ≤1.30–1.50 | Hot-finished or ERW steel tubes for structural purposes with specified yield strength (210, 240 or 310 MPa). | Trusses, columns, towers, scaffolding, handrails, structural frames |
| IS 3589 Fe 330 / Fe 410 Large-diameter welded pipe | IS 3589 · API 5L Gr. A / B (similar) | C ≤0.20–0.25 · Mn ≤1.20 | Electric-fusion or spiral-welded pipe from 168 mm to 2540 mm OD for water, sewage and low-pressure gas. | Water supply and sewage mains, penstocks, casing, structural piles |
| EN 1A / EN 1A Leaded Free-cutting | BS 970 230M07 / 230M07Pb · 11SMn30 / 11SMnPb30 (1.0715 / 1.0718) · AISI 1213 / 12L14 | C ≤0.10 · Mn 1.1 · S 0.30 (Pb 0.25 in leaded) | Sulphur (and lead) additions for very high machining speeds and excellent surface finish; not for welding or heat treatment. | Precision turned parts, bushes, studs, hydraulic fittings, screw-machine components |
| EN 3B Bright mild steel | BS 970 070M20 · C22 (1.0402) · AISI 1020 · IS 9550 20C8 (similar) | C 0.20 · Mn 0.7 | Low-carbon bright-drawn bar with good weldability and machinability; can be case-hardened. | General engineering, shafts, pins, brackets, dowels, fabricated parts |
| EN 8 / EN 8D Medium carbon | BS 970 080M40 · C40 (1.0511) · AISI 1040 · IS 40C8 · S40C | C 0.40 · Mn 0.8 | Unalloyed medium-carbon steel, tensile about 550 MPa min. normalised; can be induction or flame hardened. EN 8D is the bright-drawn version. | Shafts, studs, bolts, axles, gears, keys, general engineering |
| ST 37 / S235JR Structural | DIN St 37-2 · EN 10025 S235JR (1.0038) · IS 2062 E250 (similar) | C ≤0.17 · Mn ≤1.40 | European general structural steel with yield ≥235 MPa and tensile 360–510 MPa; good weldability and formability. | Structural sections, plates, tubes, welded frames, general fabrication |
| ST 52.3 / S355J2 High-strength structural | DIN St 52-3 · EN 10025 S355J2 (1.0577) · IS 2062 E350 (similar) | C ≤0.20 · Mn ≤1.60 · Si ≤0.55 | Structural steel with yield ≥355 MPa and impact toughness at −20 °C; good weldability; also as hydraulic cylinder tube (E355). | Cranes, bridges, earth-moving equipment, hydraulic cylinder tubes, heavy fabrication |
| IS 1079 / IS 513 HR / CR sheet | IS 1079 HR1–HR4 (hot rolled) · IS 513 CR1–CR5 (cold rolled) · DC01–DC04 (similar) | C ≤0.10–0.15 · Mn ≤0.50–0.60 | Low-carbon sheet and strip in drawing and deep-drawing qualities; smooth CR surface suitable for painting and plating. | Panels, enclosures, pressings, automotive and appliance components, ducting |
MS chequered plates, angles, channels, beams and flats are supplied to IS 2062 E250; bright bars to IS 9550. Galvanised sheets and pipes are available on request.
Steels alloyed with chromium, nickel, molybdenum and manganese for strength, toughness and high-temperature performance. Through-hardening grades (EN 19, EN 24) are used hardened and tempered; case-hardening grades (20MnCr5, EN 353, 8620) are carburised for a hard surface over a tough core; Cr-Mo grades (P11, P22, P91) resist creep in steam and refinery service. See the Alloy Steel page.
| Grade | Equivalents | Nominal Composition | Key Properties | Typical Applications |
|---|---|---|---|---|
| EN 19 / 4140 Cr-Mo, through-hardening | BS 970 709M40 · 42CrMo4 (1.7225) · AISI 4140 · IS 40Cr1Mo28 · SCM 440 | C 0.40 · Cr 1.05 · Mo 0.25 · Mn 0.8 | High tensile strength with good toughness and fatigue resistance; commonly supplied in T condition (850–1000 MPa) or annealed. | Shafts, gears, spindles, oil & gas tools, high-tensile bolts (B7 studs), hydraulic rods |
| EN 24 / 4340 Ni-Cr-Mo, through-hardening | BS 970 817M40 · 34CrNiMo6 (1.6582, similar) · AISI 4340 · IS 40Ni2Cr1Mo28 · SNCM 439 | C 0.40 · Ni 1.5 · Cr 1.2 · Mo 0.27 | Very high tensile strength and toughness in large sections; hardened & tempered up to about 1300 MPa; good hardenability. | Heavy-duty shafts, crankshafts, connecting rods, gears, axles, aerospace and defence parts |
| EN 31 / 52100 Bearing steel | BS 970 535A99 · 100Cr6 (1.3505) · AISI 52100 · IS 103Cr1 · SUJ 2 | C 1.0 · Cr 1.4 · Mn 0.35 | High-carbon chromium steel hardening to about 60–64 HRC; excellent wear and rolling-contact fatigue resistance. | Ball and roller bearings, bearing races, gauges, punches, rollers, bushes |
| EN 36 / EN 36C Ni-Cr, case-hardening | BS 970 655M13 / 832M13 · 14NiCr14 (1.5752) · AISI 3310 (similar) · SNC 815 | C 0.13 · Ni 3.4 · Cr 0.85 | High-nickel carburising steel giving a very tough core under a hard case; retains toughness in large sections. | Heavy-duty gears, camshafts, crown wheels, pinions, aircraft and truck transmission parts |
| EN 353 Ni-Cr-Mo, case-hardening | BS 970 815M17 · 17NiCrMo6-4 (1.6566, similar) · IS 15Ni4Cr1 (similar) | C 0.17 · Ni 1.45 · Cr 1.0 · Mo 0.15 | Carburising steel with high core strength and good hardenability; widely used in Indian gear manufacture. | Gears, pinions, shafts, cams, heavy-duty transmission parts |
| SAE 8620 Ni-Cr-Mo, case-hardening | AISI 8620 · 20NiCrMo2-2 (1.6523) · BS 805M20 (EN 362) · SNCM 220 | C 0.20 · Ni 0.55 · Cr 0.5 · Mo 0.2 | Versatile carburising steel with a tough core and hard, wear-resistant case; good machinability. | Gears, ring gears, camshafts, king pins, chain components, fasteners |
| 16MnCr5 Mn-Cr, case-hardening | W.Nr. 1.7131 · SAE 5115 · IS 16Mn5Cr4 · SCr 415 | C 0.16 · Mn 1.15 · Cr 0.95 | Case-hardening steel with good machinability and surface hardness after carburising. | Small and medium gears, piston pins, shafts, cams |
| 20MnCr5 Mn-Cr, case-hardening | W.Nr. 1.7147 · SAE 5120 · IS 20Mn5Cr4 · SCr 420 | C 0.20 · Mn 1.25 · Cr 1.15 | Higher hardenability than 16MnCr5 for larger sections; high core strength. | Automotive and industrial gears, crown wheels, shafts, spindles |
| SAE 4130 Cr-Mo, through-hardening | AISI 4130 · 25CrMo4 (1.7218) · 30CrMo4 · SCM 430 | C 0.30 · Cr 0.95 · Mo 0.2 | Lower carbon than 4140 for better weldability while keeping good strength and toughness after H&T; also as seamless tube. | Oil-tool components, aircraft tubing and structures, pressure vessels, welded frames |
| EN 41B Cr-Al-Mo, nitriding | BS 970 905M39 · 41CrAlMo7-10 (1.8509) · SACM 645 | C 0.39 · Cr 1.6 · Al 1.1 · Mo 0.2 | Nitriding steel developing a very hard, wear-resistant surface (about 900–1100 HV) with minimal distortion. | Nitrided shafts, spindles, extruder screws and barrels, cams, liners |
| EN 47 Cr-V, spring steel | BS 970 735A51 · 51CrV4 (1.8159) · AISI 6150 · IS 50Cr4V2 · SUP 10 | C 0.50 · Cr 0.95 · Mn 0.8 · V ≥0.15 | Spring steel with high fatigue strength and toughness after hardening & tempering. | Leaf and coil springs, torsion bars, highly stressed gears and shafts |
| A335 P11 / A213 T11 1¼Cr-½Mo · Pipe & tube | ASTM A335 P11 · UNS K11597 · 13CrMo4-5 (1.7335) · STPA 23 | Cr 1.25 · Mo 0.5 · C ≤0.15 · Si 0.5–1.0 | Creep-resisting Cr-Mo steel for service up to about 550 °C; good weldability with preheat; tensile ≥415 MPa. | Superheater and reheater tubes, refinery furnace tubes, steam headers and piping |
| A335 P22 / A213 T22 2¼Cr-1Mo · Pipe & tube | ASTM A335 P22 · UNS K21590 · 10CrMo9-10 (1.7380) · STPA 24 | Cr 2.25 · Mo 1.0 · C ≤0.15 | Higher Cr-Mo content for creep strength to about 580 °C and resistance to hydrogen attack; tensile ≥415 MPa. | High-pressure steam lines, hydrocrackers, reformer piping, boiler tubes |
| A335 P91 / A213 T91 9Cr-1Mo-V · Pipe & tube | ASTM A335 P91 · UNS K90901 · X10CrMoVNb9-1 (1.4903) · STPA 28 | Cr 9 · Mo 1 · V 0.2 · Nb 0.08 · N 0.05 | Creep-strength-enhanced ferritic steel for high-pressure, high-temperature steam up to about 600 °C; needs controlled heat treatment and welding. | Supercritical boiler tubes and headers, main steam piping, high-temperature refinery lines |
| A182 F11 / F22 / F5 Cr-Mo forgings | ASTM A182 / ASME SA182 · F11 (K11572) · F22 (K21590) · F5 (K41545) · matching A234 WP11 / WP22 / WP5 fittings | F11: Cr 1.25 Mo 0.5 · F22: Cr 2.25 Mo 1 · F5: Cr 5 Mo 0.5 | Forged flanges, fittings and valve parts matching Cr-Mo pipe grades for high-temperature, hydrogen and sulphide-bearing service; tensile ≥485 MPa (Cl. 2). | Refinery and petrochemical flanges, olets and fittings, power-plant piping components |
| A387 Gr. 11 / 22 Cr-Mo pressure-vessel plate | ASTM A387 / ASME SA387 Cl. 2 · 13CrMo4-5 / 10CrMo9-10 · EN 10028-2 | Gr. 11: Cr 1.25 Mo 0.5 · Gr. 22: Cr 2.25 Mo 1 | Chromium-molybdenum plate for elevated-temperature pressure vessels; Cl. 2 tensile 515–690 MPa, yield ≥310 MPa. | Reactors, hydrocracker vessels, heat-exchanger shells, boiler drums |
Also available on request: EN 16, EN 18, EN 9, 30MnCr5, 42CrMo4 QT plates and alloy steel fasteners to ASTM A193 B7 / A194 2H. Indian IS 1570 / IS 5517 designations are supplied against the EN / SAE grades above.
High-carbon alloy steels designed to be hardened for cutting, forming and moulding. Cold-work grades (D2, D3, D6, A2, O1) prioritise wear resistance; hot-work grades (H11, H13, DB6) resist thermal fatigue and softening; mould steel P20 is supplied pre-hardened, ready to machine; valve steels EN 52 and 21-4N resist heat and scaling. See the Tool & Die Steel page.
| Grade | Equivalents | Nominal Composition | Key Properties | Typical Applications |
|---|---|---|---|---|
| D2 (HCHCr) Cold work · Air hardening | W.Nr. 1.2379 · X153CrMoV12 · BD2 · SKD 11 · IS XT160Cr12 (similar) | C 1.55 · Cr 12 · Mo 0.8 · V 0.9 | High-carbon high-chromium, air-hardening; high wear resistance with better toughness than D3. Working hardness 58–62 HRC. | Blanking and forming dies, punches, thread-rolling dies, shear blades, gauges, cold rolls |
| D3 (HCHCr) Cold work · Oil hardening | W.Nr. 1.2080 · X210Cr12 · BD3 · SKD 1 | C 2.1 · Cr 12 | Highest wear resistance of the HCHCr family; oil-hardening. Working hardness 58–64 HRC. | Long-run blanking dies, drawing dies, brick moulds, shear blades, deep-drawing tools |
| D6 Cold work · W-bearing | W.Nr. 1.2436 · X210CrW12 · BD6 · SKD 2 | C 2.1 · Cr 12 · W 0.7 | D3 with a tungsten addition for extra abrasion resistance and hardness retention; oil hardening. Working hardness 58–64 HRC. | Blanking and punching tools, thread-rolling dies, cold rolls, measuring tools, plastic moulds |
| A2 Cold work · Air hardening | W.Nr. 1.2363 · X100CrMoV5 · BA2 · SKD 12 | C 1.0 · Cr 5.2 · Mo 1.1 · V 0.2 | Medium-alloy air-hardening steel with a better balance of toughness and wear resistance than D2, and minimal distortion. Working hardness 57–62 HRC. | Punches and dies, shear blades, thread-rolling dies, forming rolls, gauges |
| O1 (OHNS) Cold work · Oil hardening | AISI O1 · W.Nr. 1.2510 · 100MnCrW4 · BO1 · SKS 3 | C 0.95 · Mn 1.1 · Cr 0.55 · W 0.55 · V 0.1 | Oil-hardening, non-shrinking – minimal distortion on hardening; easy to machine in the annealed state. Working hardness 57–62 HRC. | Gauges, press tools, punches, measuring instruments, small dies, knives |
| H11 Hot work | W.Nr. 1.2343 · X38CrMoV5-1 · BH11 · SKD 6 | C 0.38 · Cr 5 · Mo 1.3 · V 0.4 · Si 1.0 | Excellent toughness and resistance to thermal shock; air hardening. Working hardness 44–52 HRC. | Forging dies, extrusion tooling and containers, die-casting dies, hot shear blades, high-strength structural parts |
| H13 Hot work | W.Nr. 1.2344 · X40CrMoV5-1 · BH13 · SKD 61 · IS XT35Cr5MoV1 (similar) | C 0.40 · Cr 5.2 · Mo 1.4 · V 1.0 · Si 1.0 | Higher vanadium than H11 for better hot-wear and thermal-fatigue resistance; the most widely used hot-work steel. Working hardness 44–52 HRC. | Aluminium and zinc die-casting dies, extrusion dies, hot-forging tools, plastic moulds |
| P20 / P20+Ni Plastic mould | W.Nr. 1.2311 / 1.2738 · 40CrMnMo7 / 40CrMnNiMo8-6-4 | C 0.40 · Cr 1.9 · Mn 1.5 · Mo 0.2 (+ Ni 1.0 in 1.2738) | Supplied pre-hardened (about 28–34 HRC) – machine, texture and polish without further heat treatment; P20+Ni gives uniform hardness in large blocks. | Plastic injection moulds, blow moulds, die-casting holder blocks, mould bases |
| DB6 Hot work · Die block | W.Nr. 1.2714 · 55NiCrMoV7 · BH224/5 · SKT 4 | C 0.55 · Ni 1.7 · Cr 1.1 · Mo 0.5 · V 0.1 | Nickel-chromium-molybdenum die-block steel with high toughness through large sections; supplied annealed or pre-hardened (about 36–42 HRC). | Hammer and press forging dies, die holders, bolsters, hot shear blades |
| S7 Shock resisting | AISI S7 · W.Nr. 1.2355 (similar) · 50CrMoV13-15 | C 0.50 · Cr 3.25 · Mo 1.4 · V 0.25 | Air-hardening shock-resisting steel with outstanding impact toughness and good hot hardness. Working hardness 54–58 HRC. | Chisels, punches, rivet sets, shear blades, cold and hot forming tools, plastic moulds |
| Silver Steel Precision ground bar | BS 1407 · W.Nr. 1.2210 (115CrV3, similar) · AISI W1 (similar) | C 1.15 · Cr 0.45 · Mn 0.4 · V 0.1 | High-carbon steel supplied bright ground and polished to close tolerance (h8 / h9); water or oil hardening to about 62–64 HRC. | Punches, pins, shafts, spindles, jigs and fixtures, tool-room work |
| EN 52 Valve steel · Martensitic | BS 970 401S45 · X45CrSi9-3 (1.4718) · SUH 1 · UNS S65007 | C 0.45 · Si 3.0 · Cr 9.0 · Mn 0.5 | Silchrome valve steel with good resistance to scaling and oxidation up to about 800 °C; hardenable to about 300 HB. | Intake valves, stems for bi-metal valves, high-temperature fasteners and shafts |
| 21-4N Valve steel · Austenitic | BS 970 349S54 · X53CrMnNiN21-9 (1.4871) · SUH 35 · UNS S63008 | C 0.53 · Mn 9 · Cr 21 · Ni 4 · N 0.4 | High-manganese austenitic valve steel with excellent hot strength, corrosion and scaling resistance; non-hardenable, age-hardens in service. | Highly stressed exhaust and intake valves, hot-gas components, high-temperature fasteners |
"HCHCr" is supplied as D2 or D3; "hot die steel" as H11 / H13 / DB6; "plastic mould steel" as P20 / P20+Ni. Other grades (D2M, O2, W-series, DIN 2714 modified) on request.
Highly alloyed tool steels that keep their hardness ("red hardness") at the temperatures reached in high-speed cutting. Tungsten (T) grades are the classic cutting steels; molybdenum (M) grades offer similar performance with better toughness and lower cost; cobalt grades (T4, T15, T42, M35, M42) add hot hardness for difficult materials; powder-metallurgy (PM) grades give a fine, uniform carbide structure. See the High Speed Steel page.
| Grade | Equivalents | Nominal Composition | Key Properties | Typical Applications |
|---|---|---|---|---|
| T1 Tungsten HSS · 18-0-1 | W.Nr. 1.3355 · HS18-0-1 · BT1 · IS XT72W18Cr4V1 · SKH 2 | C 0.75 · W 18 · Cr 4 · V 1.1 | The original 18-4-1 high speed steel; good red hardness and grindability, moderate toughness. Working hardness 63–65 HRC. | Turning, planing and slotting tools, taps, twist drills, threading dies, reamers, broaches |
| T4 Tungsten-cobalt HSS | W.Nr. 1.3255 · HS18-1-2-5 · BT4 · IS XT75W18Co5Cr4MoV1 · SKH 3 | C 0.75 · W 18 · Cr 4 · V 1.1 · Co 5 · Mo 0.65 | Cobalt addition to T1 for higher hot hardness and wear resistance in heavy roughing cuts. Working hardness 64–66 HRC. | Turning, planing and milling tools for roughing work, tool bits, form tools |
| T15 Tungsten-cobalt HSS · High V | W.Nr. 1.3202 · HS12-1-5-5 · BT15 | C 1.50 · W 12.5 · Cr 4.5 · V 5 · Co 5 | Very high vanadium and cobalt for maximum abrasion resistance and red hardness; difficult to grind. Working hardness 65–67 HRC. | Finishing and precision-cutting turning tools, form tools, tools for hard and abrasive materials |
| T42 Tungsten-cobalt HSS · Super | W.Nr. 1.3207 · HS10-4-3-10 · BT42 · IS XT125WCo10Cr4Mo4V3 · SKH 57 | C 1.25 · W 9.5 · Mo 3.6 · V 3.2 · Co 10 · Cr 4 | One of the hardest conventional high speed steels, with outstanding hot hardness for difficult-to-machine materials. Working hardness 66–68 HRC. | Roughing and finishing tools for hardened and heat-resisting alloys, tool bits, wood-working tools, highly stressed cold-work tools |
| M2 Molybdenum HSS · 6-5-2 | W.Nr. 1.3343 · HS6-5-2 · BM2 · IS XT87W6Mo5Cr4V2 · SKH 51 | C 0.90 · W 6.4 · Mo 5 · Cr 4.1 · V 1.8 | The most widely used general-purpose high speed steel – good balance of hardness, toughness and wear resistance. Working hardness 62–65 HRC. | Taps, twist drills, reamers, milling cutters, broaches, metal saws, wood-working and cold-work tools |
| M3 Class 2 Molybdenum HSS · High V | W.Nr. 1.3344 · HS6-5-3 · BM4 (similar) · SKH 53 | C 1.20 · W 6.4 · Mo 5.1 · Cr 4.3 · V 3.3 | Higher carbon and vanadium than M2 for improved wear resistance and hardness retention. Working hardness 63–66 HRC. | Broaches, reamers, milling cutters, taps, form tools, cold-work tooling for abrasive materials |
| M35 Molybdenum-cobalt HSS | W.Nr. 1.3243 · HS6-5-2-5 · BM35 · IS XT90W6Co5Mo5Cr4V2 · SKH 55 | C 0.92 · W 6.4 · Mo 5 · Cr 4.1 · V 1.9 · Co 4.8 | M2 with 5% cobalt for higher hot hardness – the standard choice for stainless and high-tensile steels. Working hardness 64–66 HRC. | Turning and planing tools, milling cutters, hobs, broaches, taps, twist drills, cold-work tools |
| M42 Molybdenum-cobalt HSS · Super | W.Nr. 1.3247 · HS2-10-1-8 · BM42 · IS XT110Mo10Co8Cr4W2 · SKH 59 | C 1.10 · Mo 9.5 · W 1.5 · Cr 3.9 · V 1.2 · Co 8 | High-cobalt molybdenum grade hardening to 67–69 HRC with excellent red hardness and good grindability for its hardness. | Milling cutters, twist drills, taps, broaches, end mills for hard and heat-resisting materials, cold-work tools |
| ASP 23 / ASP 2023 PM HSS | W.Nr. 1.3395 · HS6-5-3 PM · similar to M3:2 PM | C 1.28 · W 6.4 · Mo 5 · Cr 4.2 · V 3.1 | Powder-metallurgy grade with fine, evenly distributed carbides – higher toughness, dimensional stability and grindability than conventional M3:2. Working hardness 60–65 HRC. | Blanking and fine-blanking tools, cold-forming dies, knives, broaches, milling tools |
| ASP 30 / ASP 2030 PM HSS · Cobalt | W.Nr. 1.3294 · HS6-5-3-8 PM | C 1.28 · W 6.4 · Mo 5 · Cr 4.2 · V 3.1 · Co 8.5 | Cobalt-bearing PM grade combining high hot hardness with the toughness of a PM structure. Working hardness 63–67 HRC. | Gear-cutting tools (hobs, shaper cutters), end mills, taps, highly stressed cold-work tools |
| ASP 60 / ASP 2060 PM HSS · Super | HS6-7-6-10 PM | C 2.3 · W 6.5 · Mo 7 · Cr 4 · V 6.5 · Co 10.5 | Very high carbide volume for maximum wear resistance and hot hardness among PM high speed steels. Working hardness 65–69 HRC. | Tools for machining titanium, nickel alloys and hardened steels; form tools; cold-forming punches |
Indian designations follow IS 7291 (e.g. XT72W18Cr4V1 = T1, XT87W6Mo5Cr4V2 = M2). ASP® is a trademark of Erasteel. If you require any grade in any size we can arrange it; larger sizes are generally available ex-stock for faster delivery.
Copper, brass and aluminium for conductivity, machinability and light weight; nickel alloys for seawater, acids and high temperature; titanium for the best strength-to-weight ratio with near-immunity to chloride corrosion; cupro-nickels and bronzes for marine and bearing service. See the Non-Ferrous Metals page.
| Grade | Equivalents | Nominal Composition | Key Properties | Typical Applications |
|---|---|---|---|---|
| Copper C11000 ETP copper | Cu-ETP · CW004A · 2.0065 · IS 191 ETP | Cu ≥99.90 | Very high electrical conductivity (~100% IACS) and thermal conductivity; easily formed and brazed. | Busbars, earthing strips, electrical contacts, heat-transfer equipment, roofing |
| Copper C10100 / C12200 OFE · DHP copper | Cu-OFE (CW009A) · Cu-DHP (CW024A) · 2.0040 / 2.0090 | Cu ≥99.99 (OFE) · Cu ≥99.90 + P 0.015–0.04 (DHP) | Oxygen-free copper for vacuum and high-purity electrical use; phosphorus-deoxidised copper is weldable and brazeable without embrittlement. | Vacuum and electronic parts (OFE); plumbing, refrigeration and medical-gas tubes, heat exchangers (DHP) |
| Brass C36000 Free-cutting brass | CuZn36Pb3 · CW603N · 2.0375 · IS 319 Gr. 1 | Cu 61.5 · Pb 3 · Zn bal. | Benchmark for machinability among copper alloys; good corrosion resistance. | Turned components, valve bodies, plumbing fittings, fasteners, inserts |
| Brass C26000 70/30 cartridge brass | CuZn30 · CW505L · 2.0265 · IS 410 CuZn30 | Cu 70 · Zn 30 | Excellent cold formability and ductility; good strength; bright finish. | Deep-drawn parts, radiator cores, cartridge cases, lamp and hardware components |
| Naval Brass C46400 CuZn39Sn1 | CW719R · CuZn39Sn1 · 2.0530 | Cu 60 · Zn 39 · Sn 0.75 | Tin addition improves dezincification and seawater corrosion resistance; good strength and hot workability. | Marine hardware, propeller shafts, condenser plates, valve stems, tube sheets |
| Aluminium 6061 Al-Mg-Si · T6 | UNS A96061 · EN AW-6061 · AlMg1SiCu · 3.3211 · IS 65032 | Mg 1.0 · Si 0.6 · Cu 0.28 · Cr 0.2 | Versatile heat-treatable structural alloy; tensile about 310 MPa in T6; good weldability, machinability and corrosion resistance. | Structural frames, machined parts, fixtures, marine fittings, pneumatic components |
| Aluminium 6082 Al-Si-Mg-Mn · T6 (HE30) | UNS A96082 · EN AW-6082 · AlSi1MgMn · 3.2315 · BS HE30 · IS 64430 | Si 1.0 · Mg 0.9 · Mn 0.7 | Highest strength of the common 6xxx alloys (tensile about 340 MPa in T6); good machinability and corrosion resistance. | Highly stressed structures, bridges, cranes, transport components, machined blocks |
| Aluminium 7075 Al-Zn-Mg-Cu · T6 | UNS A97075 · EN AW-7075 · AlZn5.5MgCu · 3.4365 | Zn 5.6 · Mg 2.5 · Cu 1.6 · Cr 0.23 | One of the strongest aluminium alloys (tensile about 570 MPa in T6); excellent machinability; lower corrosion resistance than 6xxx. | Aerospace parts, jigs and fixtures, moulds, high-stress machined components |
| Nickel 200 / 201 Commercially pure nickel | UNS N02200 / N02201 · W.Nr. 2.4066 / 2.4068 | Ni ≥99.0 · C ≤0.15 (201: ≤0.02) | Excellent resistance to caustic alkalis and reducing environments; magnetic; 201 (low carbon) for service above 315 °C. | Caustic soda evaporators, food-processing equipment, electronic and electroplating components |
| Monel 400 Ni-Cu | UNS N04400 · W.Nr. 2.4360 · NiCu30Fe | Ni ≥63 · Cu 31 · Fe ≤2.5 | Excellent resistance to seawater, hydrofluoric acid and alkalis; tough over a wide temperature range. | Marine engineering, pumps and valves, HF-acid plants, heat exchangers |
| Monel K-500 Ni-Cu · Age-hardening | UNS N05500 · W.Nr. 2.4375 · NiCu30Al | Ni ≥63 · Cu 30 · Al 2.7 · Ti 0.6 | Corrosion resistance of Monel 400 with much higher strength and hardness after age-hardening (tensile about 1000 MPa). | Pump shafts, impellers, oil-well tools, springs, marine fasteners |
| Inconel 600 Ni-Cr-Fe | UNS N06600 · W.Nr. 2.4816 · NiCr15Fe | Ni ≥72 · Cr 15.5 · Fe 8 | Resists oxidation, carburisation and chloride stress-corrosion cracking; good strength at high temperature. | Furnace muffles, heat-treatment baskets, chemical and food processing, nuclear components |
| Inconel 625 Ni-Cr-Mo-Nb | UNS N06625 · W.Nr. 2.4856 · NiCr22Mo9Nb | Ni ≥58 · Cr 21.5 · Mo 9 · Nb 3.6 | High strength without age-hardening; exceptional pitting, crevice and seawater corrosion resistance; service from cryogenic to 980 °C. | Marine and offshore hardware, chemical plants, aerospace ducting, flue-gas systems |
| Inconel 718 Precipitation-hardening | UNS N07718 · W.Nr. 2.4668 · NiCr19Nb5Mo3 | Ni 52.5 · Cr 19 · Nb 5.1 · Mo 3 · Ti 0.9 · Fe bal. | Age-hardenable for very high strength up to about 650 °C; good weldability. | Gas-turbine and aerospace parts, high-strength fasteners, oil-tool components |
| Incoloy 800 / 800H Ni-Fe-Cr · Heat resisting | UNS N08800 / N08810 · W.Nr. 1.4876 / 1.4958 · X10NiCrAlTi32-21 | Ni 32 · Cr 21 · Fe bal. · Al + Ti 0.3–1.2 | Resists oxidation, carburisation and sulphidation at high temperature; 800H has controlled grain size for creep strength above 600 °C. | Furnace components, heat-exchanger and reformer tubes, petrochemical furnace piping |
| Incoloy 825 Ni-Fe-Cr-Mo-Cu | UNS N08825 · W.Nr. 2.4858 · NiCr21Mo | Ni 42 · Cr 21.5 · Mo 3 · Cu 2.2 · Ti 0.9 · Fe bal. | Excellent resistance to sulphuric and phosphoric acids, chloride stress-corrosion cracking and pitting; stabilised against sensitisation. | Acid-plant piping, pickling equipment, oil & gas downhole tubing, pollution-control equipment |
| Hastelloy C-276 Ni-Mo-Cr | UNS N10276 · W.Nr. 2.4819 · NiMo16Cr15W | Mo 16 · Cr 15.5 · W 3.75 · Fe 5.5 · Ni bal. | Outstanding resistance to wet chlorine, hypochlorite, ferric and cupric chlorides and strong oxidisers. | Chemical processing, pollution-control and FGD systems, pulp bleaching, waste treatment |
| Hastelloy C-22 Ni-Cr-Mo-W | UNS N06022 · W.Nr. 2.4602 · NiCr21Mo14W | Cr 21 · Mo 13.5 · W 3 · Fe 3 · Ni bal. | Versatile resistance in both oxidising and reducing media; excellent against pitting and crevice corrosion. | Pharmaceutical and chemical reactors, scrubbers, pickling equipment |
| Titanium Grade 2 Commercially pure | UNS R50400 · W.Nr. 3.7035 · Ti2 | Ti ≥99 · Fe ≤0.30 · O ≤0.25 | Excellent corrosion resistance in seawater and oxidising acids; good formability and weldability; tensile ≥345 MPa. Sheets 1–25 mm and tubes OD 6–25 mm regularly stocked. | Heat exchangers, condensers, chemical process equipment, desalination, anodes |
| Titanium Grade 5 Ti-6Al-4V | UNS R56400 · W.Nr. 3.7165 · TiAl6V4 | Al 6 · V 4 · Ti bal. | High-strength titanium alloy (tensile ≥895 MPa) with low density; heat-treatable. | Aerospace structures, medical implants, high-performance fasteners, motorsport |
| Cupro-Nickel 90/10 CuNi10Fe1Mn | UNS C70600 · CW352H · 2.0872 · IS 1545 (similar) | Cu 88.5 · Ni 10 · Fe 1.4 · Mn 0.8 | Excellent seawater corrosion and biofouling resistance; good thermal conductivity and weldability. | Seawater piping, condenser and heat-exchanger tubes, desalination plants, ship systems |
| Cupro-Nickel 70/30 CuNi30Mn1Fe | UNS C71500 · CW354H · 2.0882 | Cu 68.5 · Ni 30 · Fe 0.6 · Mn 0.8 | Higher strength and resistance to high-velocity seawater than 90/10. | Condenser tubes, feedwater heaters, offshore firewater and seawater systems |
| Aluminium Bronze AB2 Nickel-aluminium bronze | BS 1400 AB2 · EN CuAl10Fe5Ni5 (CC333G) · UNS C95500 / C63000 (similar) | Cu bal. · Al 9.5 · Ni 5 · Fe 5 | High strength (tensile about 640 MPa), excellent wear and seawater corrosion resistance, resists cavitation. | Pump impellers and bodies, valve seats, bushes, gears, marine propellers, wear rings |
| Gunmetal LG2 Leaded gunmetal | BS 1400 LG2 · EN CuSn5Zn5Pb5 (CC491K) · UNS C83600 · IS 318 Gr. 2 | Cu 85 · Sn 5 · Zn 5 · Pb 5 | Good machinability, pressure tightness and bearing properties; corrosion resistant in water and steam. | Bushes, bearings, valve and pump bodies, pipe fittings, glands |
| Phosphor Bronze PB1 / C51000 Tin bronze | BS 1400 PB1 · CuSn5 (CW451K) / CuSn10-P (CC481K) · UNS C51000 / C90700 | Cu bal. · Sn 5–10 · P 0.1–0.4 | High fatigue strength, elasticity and wear resistance; good corrosion resistance; excellent bearing properties in cast form. | Springs, bushes, bearings, worm wheels, electrical connectors, gears |
Inconel®, Monel® and Incoloy® are trademarks of Special Metals Corporation; Hastelloy® is a trademark of Haynes International. Material is supplied to the UNS number and specification on your order. Lead, zinc, tin and beryllium copper are available on request.
This page covers our most-requested grades. As importers and stockholders we supply ferrous and non-ferrous metals in any grade & size – send your requirement and our team will confirm availability, equivalents, size range and price.
A starting point for common requirements. Final selection should consider the full service conditions – our team can help.
316L · Duplex 2205 · Super Duplex 2507 · Cu-Ni 90/10 · Monel 400 · Titanium Gr 2
SS 310S · SS 309S · SS 321 · Incoloy 800H · Inconel 600 / 625
SS 904L · Incoloy 825 · Hastelloy C-276 / C-22 · Inconel 625 · Titanium Gr 2
EN 19 / 4140 · EN 24 / 4340 · C45 · EN 8 (lighter duty)
20MnCr5 · 16MnCr5 · EN 353 · SAE 8620 · EN 36
EN 31 / 52100 · Gunmetal LG2 · Phosphor Bronze
D2 · D3 · D6 · A2 · O1 (OHNS) · Silver Steel
H13 · H11 · DB6 · S7
P20 / P20+Ni (pre-hardened) · H13 · SS 420
M2 (general) · M35 (stainless) · M42 / T42 (hard materials) · ASP 23 / 30 (PM)
IS 2062 E250 / E350 · S355J2 · IS 1239 / IS 1161 tubes · A36
A333 Gr. 6 · A350 LF2 · A420 WPL6 · SS 304L / 316L
SA 516 Gr. 70 · A106 Gr. B · SA 210 · P11 / P22 / P91 · A387
EN 52 (inlet) · 21-4N (exhaust) · EN 47 (springs) · EN 24
EN 1A Leaded · SS 303 / 416 · Brass C36000
Copper C11000 / C10100 · Aluminium 6061 / 6082
Titanium Gr 5 · Aluminium 7075 · Aluminium 6082
PVC-coated SS 304 & 316 sheets – our speciality for kitchens, pharma and architectural work
Send us the product, grade, size, quantity and delivery location – our team replies with stock status and a competitive quote, usually the same working day.